Hi, I have printed a small holder for a Bowden tube to print from my filament dryer outside of the enclosure, but the filament coming out of the tube is tensioned and I don’t know if it will cause problems later. Is this fine to keep or how can I fix this? This i a Ender 3 V3 SE btw.

  • kata1yst@sh.itjust.works
    link
    fedilink
    English
    arrow-up
    4
    ·
    21 hours ago

    I’ll say that it can lead to uneven extrusion and even skipped steps on your extruder. How much, and how much that amount matters is entirely dependant on the setup and your workflow.

    There are a few 3D printed solutions to keep filament tension neutral using a buffer system. It’s not a bad idea to check out some of them.

  • JohnEdwa@sopuli.xyz
    link
    fedilink
    English
    arrow-up
    2
    ·
    21 hours ago

    What type of a spool holder you have in the dryer? It might be a good idea to get some bearings in there to help the spool spin as freely as possible.

    • Imgonnatrythis@sh.itjust.works
      link
      fedilink
      English
      arrow-up
      2
      ·
      19 hours ago

      Recommend this. Have a similar setup and you can 3d print spools and order bearings for them. That being said my direct drive filament feeder on my prusa is quite strong. As long as you make smooth curves with your bowden tube it should be ok.

  • Boomkop3@reddthat.com
    link
    fedilink
    English
    arrow-up
    2
    ·
    21 hours ago

    That should be fine, I’ve printed tens of kilograms pulling the filament around a sharp corner. As long as it’s dry, pla can handle quite a bit of abuse. And it’s unlikely to damage your printer or dryer.

    In the worse case you might have some dust buildup, keep it clean

    • papalonian@lemmy.world
      link
      fedilink
      English
      arrow-up
      1
      ·
      16 hours ago

      Re: dry. I’m convinced PLA doesn’t care about moisture. Watched a video of a guy that soaked a roll in a tub of water overnight, then printed off the roll with it still in the tub. Looked exactly the same as it did before the soak.

      Mileage may vary of course but ever since then I’ve been leaving my PLA out and it’s never once given me trouble (the infused ones a little bit).

      • Boomkop3@reddthat.com
        link
        fedilink
        English
        arrow-up
        1
        ·
        15 hours ago

        I’ve had filament sit for months before it started getting brittle. But it does get very brittle. At least the stuff I have bought so far has

  • nous@programming.dev
    link
    fedilink
    English
    arrow-up
    1
    ·
    21 hours ago

    It might. Depending on how much tension there is. Too much and it will cause the filament to slip in the extruder causing under extrusion. If you are not seeing signs of under extrusion then you are fine for now - but that might change if you change filament or anything else. I would try to lower how much tension the filament is under to avoid problems in the future. Otherwise it would be something to keep in mind if you do start seeing signs of under extrusion.

      • nous@programming.dev
        link
        fedilink
        English
        arrow-up
        1
        ·
        12 hours ago

        It could be a tight bend in the line somewhere - make sure there are no tight bends. Otherwise if it is the tube then get a thicker tube.